Professional Documents
Culture Documents
(https://theconstructor.org/)
Concrete air entrainment is not an easy process since it is influence by several factors.
These factors shall be properly investigated to be able to obtain designated air
entrainment.
3. Coarse aggregates
4. Temperature of concrete
Increase of water content in the mixture will lead to increase concrete air content and
vice versa. This is because the increase of water content would increase fluid mixture
into which air bubbles could be integrated easily through mixing operation.
Hard water such as well or quarry water, which contain minerals, would reduce air
content if they are used to dilute air entraining admixture.
https://theconstructor.org/concrete/factors-affecting-concrete-air-content/21807/?utm_source=pushengage&utm_medium=push_notification&utm_campaign=pushenga
6/11/2018 What Factors Affects Air Content of Concrete?
Air entrainment will be carried out easily as the percentage of fine aggregate is
increased. Fine aggregate sizes ranges from sieve No. 30 to sieve No. 100 will create
small voids that can contain air bubbles.
However, other fine aggregate sizes will require greater quantity of air entraining
admixture to reach the same air content.
For constant amount of air entraining admixture, the increase of temperature will lead
to decline concrete air content. So, if temperature varies considerably during mixture
production, it would be required to adjust air entraining admixture to achieve
designated air content.
Temperature reduction from 21C to 5C will increase air content by 40% whereas
increase of temperature from 21C to 38C will decline air content by 25%.
Air content increase by mixing for up to 15 minutes and mixing beyond this time will
decrease air content. Entrained air will vary with type, physical condition, speed of the
mixer and quantity of concrete that is being mixed.
Seriously worn mixer will increase difficulty of air entrainment operation. Similarly,
mixer with significant amount of hardened concrete buildup on mixer blades or in a
drum increase air entrainment operation.
There are number of admixtures that have air entraining capacity for example
retarding admixture and water reducing admixture. So, smaller quantity of air
entraining admixture will be needed when these admixtures are also provided in the
mixture.
Air content of concrete reduces with the increase of cement fineness. For the same air
content, concrete produced using Type I cement need considerably lesser quantity of
air entrainment admixture compare with concrete made with Type III cement.
Air content reduces as the fineness or surface area of fly as increases. Increase of fly
ash per unit concrete reduces air content of concrete and increase in fly ash carbon
content reduces concrete air content.
Vibration reduces concrete air content. For example, half of air content will be lost if
vibration is applied for more than three minutes.
https://theconstructor.org/concrete/factors-affecting-concrete-air-content/21807/?utm_source=pushengage&utm_medium=push_notification&utm_campaign=pushenga